Reference illustration — produced to your drawing
Rivets
Lockbolts
Lockbolts are two-piece fasteners with a grooved pin and a collar that is swaged into the pin grooves under load. The swaged joint gives consistent clamp force and strong resistance to vibration loosening.
Used in trucks, trailers, rail, and heavy equipment where a bolted joint must not loosen in service. Buyers are vehicle and equipment manufacturers replacing rivets or high-grade bolts.
This is one of the types covered by our Custom Fasteners page — materials, tolerances, lot sizes and how we quote the whole family.
Typical price US$0.20 – US$3.50 per piece at 100–1,000 pcs — final price depends on material, tolerance and finish, and is confirmed by quote.
Standard
To your drawing
Size range
Pin diameter 4.8 – 19.0 mm · 3/16 – 3/4 in
MOQ
From 50 pcs
Lead time
Samples 5–10 days
What we produce
- Two-piece pin and swaged collar system
- Annular grooves on the pin lock the collar
- Steel or alloy steel 4140 pin with steel or aluminium collar
- Round, truss, or countersunk pin heads
- Set with a lockbolt installation tool
- Metric and inch pin diameters
Specification notes
- Collar swaged to a set grip length
- No re-torquing needed after installation
- Pin and collar supplied as a matched pair
Specifications
Every line below is a starting point, not a limit. Non-standard sizes, special threads and unusual materials are what we do — send the drawing and we confirm what fits.
| Size range | Pin diameter 4.8 – 19.0 mm · 3/16 – 3/4 in |
|---|---|
| Threads | Not applicable |
| Head / geometry | Round, truss, or countersunk pin head; collar swaged by tool, no drive recess |
| Materials | Stainless steel 301 / 303 / 304 / 304L / 316 / 316L / 410 / 416 / 17-4PH · carbon steel 1045 / 1215 / 12L14 · alloy steel 4130 / 4140 · aluminium 2024 / 5052 / 6061 / 7075 · brass · bronze · copper · titanium |
| Finishes | As machined · black oxide · zinc plating · nickel plating · chrome plating · anodizing · passivation (through our vetted partner network) |
| Precision | ±0.01 mm on features that locate, seal or fit; ISO 2768-m for general dimensions |
| Marking | Head marking, grade marking or your own identification mark per drawing |
| Documents | Material certificate (MTR) with every batch, plus pre-shipment photos before dispatch |
| MOQ | From 50 pieces per type and material · samples from 1 piece |
| Sample lead time | 5–10 days |
| Production lead time | 25–35 days after sample approval |
| Quote | Within 24 hours, with DFM feedback |
Other rivets we manufacture
See all 179 part types →Send us the drawing
We reply within 24 hours with DFM feedback, a process route and a price. Samples from 1 piece, production from 50 pieces, shipped from Qidong City, Jiangsu Province, China.