Eye Bolts

Reference illustration — produced to your drawing

Bolts

Eye Bolts

A bolt with a closed loop (eye) formed at one end and a threaded shank at the other. The eye accepts a hook, rope, or shackle for lifting and anchoring.

Used as lifting and anchor points on machinery, castings, and structures. Bought by rigging, construction, and equipment suppliers.

This is one of the types covered by our Custom Bolts page — materials, tolerances, lot sizes and how we quote the whole family.

Typical price US$0.20 – US$3.50 per piece at 100–1,000 pcs — final price depends on material, tolerance and finish, and is confirmed by quote.

Standard

ASME B18.15 / DIN 580

Size range

M6 – M48 · 1/4 – 1-1/2 in

MOQ

From 50 pcs

Lead time

Samples 5–10 days

What we produce

  • Carbon steel or stainless steel 316L
  • Forged or formed eye with threaded shank
  • Metric coarse or UNC threads
  • Hot-dip galvanized or zinc finish

Specification notes

  • Common lengths from 20 mm to 300 mm
  • Shoulder and machinery eye variants available
  • Working load depends on shank size and material

Specifications

Every line below is a starting point, not a limit. Non-standard sizes, special threads and unusual materials are what we do — send the drawing and we confirm what fits.

StandardASME B18.15 / DIN 580
Size rangeM6 – M48 · 1/4 – 1-1/2 in
ThreadsMetric coarse · UNC
Head / geometryClosed forged or formed eye at the head with a threaded shank; no drive recess
MaterialsStainless steel 301 / 303 / 304 / 304L / 316 / 316L / 410 / 416 / 17-4PH · carbon steel 1045 / 1215 / 12L14 · alloy steel 4130 / 4140 · aluminium 2024 / 5052 / 6061 / 7075 · brass · bronze · copper · titanium
FinishesAs machined · black oxide · zinc plating · nickel plating · chrome plating · anodizing · passivation (through our vetted partner network)
Precision±0.01 mm on features that locate, seal or fit; ISO 2768-m for general dimensions
MarkingHead marking, grade marking or your own identification mark per drawing
DocumentsMaterial certificate (MTR) with every batch, plus pre-shipment photos before dispatch
MOQFrom 50 pieces per type and material · samples from 1 piece
Sample lead time5–10 days
Production lead time25–35 days after sample approval
QuoteWithin 24 hours, with DFM feedback

Standard dimensions

Metric hex head bolts and screws — nominal dimensions (ISO 4014 / ISO 4017)

dPitch (mm)s (mm)k (mm)e (mm)
M50.883.58.79
M61.010411.05
M81.25135.314.38
M101.5166.417.77
M121.75187.520.03
M162.0241026.75
M202.53012.533.53
M243.0361539.98
M303.54618.750.85
M364.05522.560.79

d = nominal thread diameter · s = width across flats · k = head height · e = width across corners. Nominal values; your drawing always takes precedence.